Difference between revisions of "Hydrolysis resistance"
From www.leather-dictionary.com - The Leather Dictionary
(3 intermediate revisions by one user not shown) | |||
Line 4: | Line 4: | ||
− | The hydrolysis resistance of humid [[Leather|leather]] is [[Leather quality|tested]] over a defined period and at a certain | + | The hydrolysis resistance of humid [[Leather|leather]] is [[Leather quality|tested]] over a defined period and at a certain temperature. It determines when the leather [[Leather damages|disintegrates]] and to what extent. |
The typical surface cracking of cheaper furniture made of [[Imitation leather|imitation leather]] is also called hydrolysis. | The typical surface cracking of cheaper furniture made of [[Imitation leather|imitation leather]] is also called hydrolysis. | ||
Line 10: | Line 10: | ||
<p align=center> | <p align=center> | ||
− | [[bild:Fettkragen-01.jpg| | + | [[bild:Fettkragen-01.jpg|500px]] |
− | [[bild:Einlage-Schweiss-01.jpg| | + | </p> |
+ | <p align=center> | ||
+ | [[bild:Einlage-Schweiss-01.jpg|500px]] | ||
</p> | </p> | ||
<p align=center> | <p align=center> | ||
''Moisture from perspiration promotes the disintegration of the leather fibers: Grease collar at [[Leather clothing|leather clothing]] or sweat stains in [[Leather shoes|shoes]].''<br></p> | ''Moisture from perspiration promotes the disintegration of the leather fibers: Grease collar at [[Leather clothing|leather clothing]] or sweat stains in [[Leather shoes|shoes]].''<br></p> | ||
<p> </p> | <p> </p> | ||
− | |||
− | |||
− | |||
− | |||
== Additional information == | == Additional information == | ||
Line 26: | Line 24: | ||
− | < | + | <logoplustext /> |
− | + | ||
− | + | ||
− | + | ||
− | + | ||
− | + | ||
[[Kategorie:All Articles]] | [[Kategorie:All Articles]] | ||
[[Kategorie:Leather production]] | [[Kategorie:Leather production]] |
Latest revision as of 19:19, 20 September 2022
The hydrolysis resistance of humid leather is tested over a defined period and at a certain temperature. It determines when the leather disintegrates and to what extent.
The typical surface cracking of cheaper furniture made of imitation leather is also called hydrolysis.
Moisture from perspiration promotes the disintegration of the leather fibers: Grease collar at leather clothing or sweat stains in shoes.